Buy high-quality Inconel 718 GH4169 N07718 corrosion-resistant superalloy from the leading manufacturers. We are a factory ensuring top-notch products.
Inconel718 is an iron-nickel-chromium-based precipitation hardening deformation high-temperature alloy. The long-term use temperature range is -253 ~ 650℃, and the short-term use temperature is 800℃. It has high strength and toughness below 650℃, and is in high and low temperature environments. It has oxidation resistance and corrosion resistance, as well as excellent production and processing performance, electric welding performance and long-term mechanical stability, and its state can be solid solution treatment or precipitation hardening state. The unique formula of Inconel 718 improves the strength and corrosion resistance, and at the same time has simple machinability and ease of welding. Inconel718 alloy has been used to produce rings, blades, standard parts and structural parts in the aviation, aerospace engineering and energy industries. Similar grades GH4169, GH169 (China), NC19FeNb (France), NiCr19Fe19Nb5, Mo3 (Germany), NA 51 (UK) Inconel718, UNS NO7718 (USA) NiCr19Nb5Mo3 (ISO) Inconel 718 Chemical composition%
Ni
50-55
Cr
17-21
Fe
Bal.
Cu
≤0.3
Nb
4.75-5.5
C
≤0.08
Mn
≤0.35
Si
≤0.35
S
≤0.015
Mo
2.8-3.3
Ti
0.65-1.15
Al
0.2-0.8
P
≤0.015
B
0.006
Co
≤1
The minimum mechanical properties of Inconel 718 alloy at room temperature
Yield Strength
Tensile strength
Elongation
Brinell hardness
Mpa
Mpa
%
HB
≥550
≥965
≥30
≤363
Inconel 718 Physical properties
Density
8.24 g/cm3
Melting point
1260-1320 ℃
Inconel 718 features
A. Ease of processing B. High tensile strength, fatigue strength, creep strength and breaking strength at 700°C C. High oxidation resistance at 1000°C D. Stable chemical properties at low temperatures E. Good welding performance Inconel 718 application area Due to its high-temperature strength at 700°C, excellent corrosion resistance, and ease of processing, 718 can be widely used in various high-demand occasions. A. Steam turbine B. Liquid fuel rocket C. Low temperature engineering D. Acidic environment E. Nuclear Engineering Supply form and specification
Alloy grade
Form
Specification
Inconel718
Wire
Diameter=0.025mm~8mm
Inconel718
Flat wire
Width=0.4~40mm
Thick=0.03~2.9mm
Inconel718
Strip
width=8~250mm
ThickT=0.1~3.0mm
Inconel718
Foil
width=6~120mm
Thick=0.003~0.1mm
Inconel718
Bar
Diameter=8~100mm
Long=50~1000
Superalloy Series: GH3030 GH4145 GH4169 Hastelloy C2 Hastelloy C4 Hastelloy C276 Hastelloy X Incoloy 800H Incoloy 825 Inconel 600 Inconel 625 Inconel 718 Inconel 725 Inconel X750 Monel 400 Monel K500 Nimonic 75A Nimonic263Shijiazhuang Chengyuan Alloy Material Co., Ltd. is a high-tech enterprise specializing in the production of various alloy materials. It has an advanced and complete production line, including material smelting, surface cleaning, rolling, slitting, and a complete test process. Meet the corresponding quality inspection of different products. The company focuses on the production and supply of various electric heating alloys, expansion alloys, soft magnetic alloys, elastic alloys, high temperature alloys and all kinds of pure metals. The product forms include wire, flat wire, strip, plate, bar, foil, Seamless pipe, wire mesh, powder, etc. can meet the application needs of different customers. The various performance indicators of the product are strictly in accordance with the national standards. If customers put forward non-standard requirements, they can also be implemented by reference.Our products are widely used in heating equipment, machinery manufacturing, electric furnace production, instrumentation, household appliances, mineral mining, aerospace, petroleum and nuclear power and other industries, and have received good market feedback. Our products have stable delivery time, excellent quality, sophisticated packaging, and high repurchase rate. They are not only widely recognized in the domestic market, but also have a good reputation in the international market.* OEM manufacturer* We will deliver the goods to the warehouse of the customer's agent in any city in China.* Terms of delivery: EXW, FCA, FOB, CIF, CPT, DAP* Mode of transport: Sea, Auto, Railway, Air and Express* Payment terms: Bank Transfer, Western Union, PayPal, Alipay* Quality Certificate:In order to improve the quality of products and services, with each order we provide a quality certificate for goods, which includes measured data - chemical composition, electrical resistivity, tensile strength, elongation, melting number, etc.Cheng Yuan Alloy Material Co., LtdEmail: [email protected]Tel .: +86 13673186216+86 311 8803 3197