316L is a derivative of 18-8 type austenitic stainless steel, with 2 to 3% of Mo added. The Mo content of 316L makes this steel with excellent resistance to pitting corrosion and can be safely used in environments containing Cl- and other halogen ions. Due to its excellent corrosion resistance, it has a wide range of applications in the chemical industry. 316 and 316L stainless steels are widely used in petroleum, nitrogen, shipbuilding, chemical, construction, refinery, medical, cellulose, cryogenic, automotive, and food processing industries to plate, strip, pipe, casing, fittings, forgings, and bars. Form supply for gas installations, heat exchangers, railings, marine equipment and public transport vehicles, valves, storage tanks, pumps, radiators, food processing machinery in dairy products, catering, meat processing plants, vegetables and fruits Processing plants, stills, chimneys, steam systems, piping, pressure equipment, crystallizers, reservoirs, silos, swimming pools, boiler parts, condensers, autoclaves, reactors or condensing equipment. Heat resistance316 stainless steel has good oxidation resistance in intermittent use up to 871°C (1600F°) and continuous use up to 927C° (1700F°). In the range of 427°C-857°C (800°F-1575°F), it is best not to use 316 stainless steel continuously, but the stainless steel has good heat resistance when used continuously outside this temperature range. The carbide precipitation resistance of 316L stainless steel is better than that of 316 stainless steel, and the above temperature range can be used. Heat treatmentAnnealed in the temperature range of 1850-2050 degrees, then rapidly annealed, then rapidly cooled. 316 stainless steel cannot be hardened by heat treatment. AISI 316L Chemical Composition,%
Fe
Bal.
Ni
10.0~14.0
Cr
16.0-18.0
Mo
2.0~3.0
Mn
≤2.0
Si
≤1.0
C
≤0.3
P
≤0.045
S
≤0.03
AISI 316L Physical performance
Yield Strength
Tensile strength
Elongation
Brinell hardness
Rate of reduction in area
Density
Specific heat capacity
Mpa,≥
Mpa,≥
%,≥
HB
ψ (%)
g/cm3
20℃,KJ·kg-1K-1
175
480
40
≤187
≥50
7.98
0.502
Thermal conductivity(W·m-1·K-1)
100℃
300℃
500℃
15.1
18.4
20.9
Shijiazhuang Chengyuan Alloy Material Co., Ltd. is a high-tech enterprise specializing in the production of various alloy materials. It has an advanced and complete production line, including material smelting, surface cleaning, rolling, slitting, and a complete test process. Meet the corresponding quality inspection of different products. The company focuses on the production and supply of various electric heating alloys, expansion alloys, soft magnetic alloys, elastic alloys, high temperature alloys and all kinds of pure metals. The product forms include wire, flat wire, strip, plate, bar, foil, Seamless pipe, wire mesh, powder, etc. can meet the application needs of different customers. The various performance indicators of the product are strictly in accordance with the national standards. If customers put forward non-standard requirements, they can also be implemented by reference.Our products are widely used in heating equipment, machinery manufacturing, electric furnace production, instrumentation, household appliances, mineral mining, aerospace, petroleum and nuclear power and other industries, and have received good market feedback. Our products have stable delivery time, excellent quality, sophisticated packaging, and high repurchase rate. They are not only widely recognized in the domestic market, but also have a good reputation in the international market.* OEM manufacturer* We will deliver the goods to the warehouse of the customer's agent in any city in China.* Terms of delivery: EXW, FCA, FOB, CIF, CPT, DAP* Mode of transport: Sea, Auto, Railway, Air and Express* Payment terms: Bank Transfer, Western Union, PayPal, Alipay* Quality Certificate:In order to improve the quality of products and services, with each order we provide a quality certificate for goods, which includes measured data - chemical composition, electrical resistivity, tensile strength, elongation, melting number, etc.Cheng Yuan Alloy Material Co., LtdEmail: [email protected]Tel .: +86 13673186216+86 311 8803 3197